# Grain-oriented electrical steel: Bill of materials

Source page: https://www.materialinsights.org/products/p_grain_oriented_electrical_steel/prod-bom/

#### About these figures

Which unit, study and year the composition figures describe, and how they vary

Per tonne of finished sheet. Silicon is about 3.2% of thyssenkrupp's hot-rolled base strip (2021 production) ^[4] and about 3% in a general source, which adds about 96.5% iron and 0.5% other elements ^[9]. The EPD records 127 kg of secondary material per tonne ^[4]. Inhibitor elements such as manganese and aluminium, and the coating, are small amounts that no opened source quantifies, so they are not counted. Cores, laminations and non-oriented steel are not yet nodes.

as of 2026-11-15

#### Direct materials

The commodities and chemicals in one unit as bought, with amount, mass share, cost share and recycled content

| Material | Role | Amount in one unit | Share of the unit's mass | Recycled content |
|---|---|---|---|---|
| [Fe Iron ore](https://www.materialinsights.org/commodities/iron_ore/) | Structural | 965 kg | **96.5%** | 12.7% |
| About 96.5% iron ^[9]; the EPD records 127 kg of secondary material per tonne, calculated as 12.7% ^[4]. Iron comes from ore and from scrap. Iron ore is the nearest node, so the amount is iron content, not ore mass. |  |  |  |  |
| [Si Silicon](https://www.materialinsights.org/commodities/silicon/) | Functional | 32 kgrange 30 to 33 kg | **3.2%** | – |
| Silicon is about 3.2% of the base strip ^[4] (32 kg per tonne, calculated), about 3% in a general source ^[9], and normally below 3.30% ^[7]. It is added as silicon alloys ^[1]. |  |  |  |  |

as of 2026-11-15

#### How it is put together

The main steps from parts and materials to the finished unit

| Step | What happens | Technology | Source |
|---|---|---|---|
| Melt and cast | Steel scrap and silicon alloys are melted and cast into slabs. | – | ^[1] |
| Reheat and hot roll | Slabs are reheated to dissolve the inhibitor compounds, then hot rolled to heavy coils; hot rolling loses 3.5% of the metal. | – | ^[1] |
| Cold roll | The coil is cold rolled to final thickness; this step loses under 0.025% of the metal. | – | ^[1] |
| High-temperature anneal | Coils are held above 1,100 C for more than 10 hours; the steel is purified, the aligned crystals grow and a forsterite film forms. The whole cycle takes 4 to 6 days. | – | ^[17] |
| Coat and refine domains | The coil is trimmed again, annealed, laser treated to develop the grain orientation and coated; the best grades have their domains refined by laser. | Laser | ^[1]^[8] |
| Cut and stack | Transformer makers cut the sheet into laminations and stack them into the core. | – | ^[1] |

as of 2026-11-15

#### Technologies used to make it

The technologies used to make it, at which step
 Made with

- [Lsr Laser](https://www.materialinsights.org/technologies/laser/) Laser irradiation of the sheet surface to refine magnetic domains (domain-refined grades) One maker's HI-B LS grade is made this way ^[8]; no share of output found.

as of 2026-11-15

#### Sources

1. [Electric Grid Supply Chain Review: Large Power Transformers and High Voltage Direct Current Systems](https://www.energy.gov/sites/default/files/2022-02/Electric%20Grid%20Supply%20Chain%20Report%20-%20Final.pdf) US Department of Energy, 2022
2. [Environmental Product Declaration EPD-TKE-20240546-CBC1-EN: powercore grain oriented electrical steel](https://www.thyssenkrupp-steel.com/media/content_1/publikationen/epd/thyssenkrupp_epd_grain_oriented_electrical_steel_en_steel.pdf) thyssenkrupp Electrical Steel, programme holder Institut Bauen und Umwelt e.V. (IBU), 2025
3. [The processing, microstructure, texture, and magnetic properties of electrical steels: A review (He and Kestens, International Materials Reviews 70(5), 353-393)](https://repository.tudelft.nl/file/File_a21e848f-72b1-4ce1-9d83-8ee02186e6fb) TU Delft repository copy, 2025
4. [Grain-Oriented Electrical Steel Sheets (ORIENTCORE product page)](https://www.nipponsteel.com/en/product/electrolytic-tinplate/02.html) Nippon Steel Corporation, 2026
5. [Electrical steels](https://www.megger.com/en-gb/et-online/january-2010-(1)/electrical-steels) Megger (Electrical Times online), 2010
6. [Technologies for high-temperature batch annealing of grain-oriented electrical steel: An overview (Open Engineering 14)](https://orca.cardiff.ac.uk/170404/1/ENG-14-1-10.1515_eng-2024-0053.pdf) De Gruyter, Cardiff University repository copy, 2024

## Other sections

- [Summary](https://www.materialinsights.org/products/p_grain_oriented_electrical_steel/index.md)
- [Working](https://www.materialinsights.org/products/p_grain_oriented_electrical_steel/prod-working/index.md)
- [Use case](https://www.materialinsights.org/products/p_grain_oriented_electrical_steel/prod-use/index.md)
- [Supply chain](https://www.materialinsights.org/products/p_grain_oriented_electrical_steel/prod-supply/index.md)
- [Footprint](https://www.materialinsights.org/products/p_grain_oriented_electrical_steel/prod-footprint/index.md)
- [Evolution](https://www.materialinsights.org/products/p_grain_oriented_electrical_steel/prod-evolution/index.md)
- [Interventions](https://www.materialinsights.org/products/p_grain_oriented_electrical_steel/prod-interventions/index.md)