Material Insights · Understanding the Material World

High-temperature batteries: Energy footprint

Energy in use

The energy it uses or converts while it works, and how efficiently

Consumption
Electricity for charging, plus heat to keep the cells at about 300 C [1], or 270 to 350 C depending on the type [8]
Conversion
Electricity to chemical energy in sodium and sulphur (or nickel chloride) and back
Efficiency
80 to 85% round trip for sodium-sulphur and sodium-nickel chloride cells in DOE's comparison [8]; near 90% total energy efficiency for ZEBRA cells including heating [2]
Unit
%
Note
A NAS container gives 250 kW peak and 1.45 MWh, enough for six to eight hours of discharge [4].

as of 2026-11-12

Energy links

The energy sources and technologies it uses, holds, converts, loses or gets back

Stores
  • El Electricity Electricity drives sodium ions back across the ceramic on charging and is returned on discharge [2].
Consumes
  • Ht Heat The cells only work when hot, about 300 C, so heat must be supplied or retained [1].

as of 2026-11-12

Sources

  1. Inside Cooperative Innovation: Development and Commercialization of Sodium-Sulfur Batteries for Power Storage Hitotsubashi University Institute of Innovation Research, Case 13-01 (E. Fukushima), April 2013, 2013
  2. Molten sodium batteries: advances in chemistries, electrolytes, and interfaces Frontiers in Batteries and Electrochemistry 3 (R. C. Hill and others), doi:10.3389/fbael.2024.1369305, 2024
  3. NAS Battery: product sheet (container specifications and references), dated 02/2024 BASF Stationary Energy Storage, 2024
  4. Sodium Batteries: Technology Strategy Assessment, Findings from Storage Innovations 2030 US Department of Energy (DOE/OE-0035), 2023