Open-hearth steelmaking
A regenerative furnace melts pig iron and scrap slowly, giving steel of controlled quality.
Making materials · Metals · No. 394
- Steam and steel
- Readiness 9 of 9
- Process
A furnace that recycled its own exhaust heat made nine tenths of British and American steel until 1950.
Chart: Illustration: Open-hearth steelmaking
Where it comes from
Chart: Map of where it comes from
Friedrich and William Siemens built a furnace that stored exhaust heat in brickwork to preheat the incoming air. In 1864 Pierre and Emile Martin used one to make steel in France.
Three things to know
- The open hearth could melt any mix of molten pig iron and cold scrap, so steelworks could melt scrap as well as fresh iron.
- A heat took 12 to 18 hours, long enough for steelmakers to test the metal and adjust it before tapping.
- Oxygen steelmaking replaced it from about 1960; Russia shut its last open hearth in 2018 and India's SAIL in 2020.
The journey
- 1 ChargeMolten pig iron, cold scrap, iron ore and limestone go onto a shallow hearth
- 2 RegeneratorsBrick chambers heated by the exhaust warm the incoming air and gas
- 3 MeltingThe hot flame sweeps over the charge and melts it
- 4 RefiningOver many hours oxygen burns out carbon and limestone takes up impurities as slag
- 5 TappingSteel is sampled until it is right, then poured into ladles